Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.10 g/cc
0.112 lb/in³
Porosity 17 %
17 %
Mechanical Properties Metric English Comments
Compressive Strength 98.1 MPa
14200 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 7.00 µm/m-°C

@Temperature 1000 °C
3.89 µin/in-°F

@Temperature 1830 °F
Shrinkage 0.00 %

@Temperature 1500 °C,
Time 7200 sec
0.00 %

@Temperature 2730 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 91 %
91 %
Fe2O3 0.30 %
0.30 %
Descriptive Properties Value Comments
Main Application Carbon productor, Ammonia plant, Incinerator, Various High-temp. furnace
Refractories Under Load(2kg/?,T2?) 1,700 T2
Refractoriness (SK) 40