Chosun Refractories CSN-332N Plate Brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CSN-332N Plate Brick.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.05 - 3.15 g/cc
0.110 - 0.114 lb/in³
Porosity 7.0 - 10 %
7.0 - 10 %
Mechanical Properties Metric English Comments
Modulus of Rupture <= 0.00981 GPa

@Temperature 1400 °C
<= 1.42 ksi

@Temperature 2550 °F
Compressive Strength <= 127 MPa
<= 18500 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 75 - 80 %
75 - 80 %
Carbon, C 7.0 - 10 %
7.0 - 10 %
ZrO2 5.0 - 8.0 %
5.0 - 8.0 %
Descriptive Properties Value Comments
Remarks Spalling resistance, Oxidation resistance