China Tungsten YWR2 Tungsten Carbide with Rare Earth Additive

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YWR2 Tungsten Carbide with Rare Earth Additive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Higher wear resistance and service strength than YW2 capable of undergoing high impact load. For roughing and Semi-finishing of heat resistant steel ,hi-Mn steel, stainless steel and high alloy steel, and for processing of ordinary steel and cast iron.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 12.5 - 13.5 g/cc
0.452 - 0.488 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A >= 91
>= 91
Flexural Strength >= 1460 MPa
>= 212000 psi