China Tungsten YT770 Tungsten Carbide

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YT770 Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High toughness. wear resistance and heat shock resistance. for milling and medium speed and full-feed turning of steel, cast steel, alloy steel, stainless steel and hi-Mn steelInformation provided by China Tungsten
Physical Properties Metric English Comments
Density 12.8 - 12.95 g/cc
0.462 - 0.4678 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 91
91
Flexural Strength 1900 MPa
276000 psi