China Tungsten NT4 Titanium Carbonitride Alloy

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten NT4 Titanium Carbonitride Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Titanium carbonitride base alloy , also called cermets, with of high hardness, good red hard-ness and wear resistance, medium toughness, high  corrosion resistance to acids and alkalis and hi-temperature oxidation resistance, and low density, used as tool materials for manufacturing cars, tractors and other engine industries; bet for cutting of carbon steel, low and medium alloy steels, and gray cast iron; of high cutting speeds, long tool life and high surface finish also used in seal rings and housings in manufacturing of chemical engineering equipment.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 6.50 g/cc
0.235 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 91
91
Flexural Strength 1600 MPa
232000 psi