Material Notes:
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityApplications:Chemical processing – production, storage and transfer of corrosive fluidsElectronics – protective sheathing, plenum and wiring insulationSemi-conductor industryFood stuff and Healthcare industriesTransportation – fuel line and pipe, thermoformed body componentsInformation provided by Arkema Inc.
Physical Properties Metric English Comments
Bulk Density 0.288 g/cc
0.0104 lb/in³
Particle Size 5.0 µm
5.0 µm
Loosely agglomerated
Particle Mesh Size 14 Mesh
14 Mesh
Viscosity 400000 - 800000 cP

@Shear Rate 100 1/s,
Temperature 232 °C
400000 - 800000 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Melt Flow 19 - 35 g/10 min

@Load 3.80 kg,
Temperature 232 °C
19 - 35 g/10 min

@Load 8.38 lb,
Temperature 450 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 165 - 172 °C
329 - 342 °F