| Category | Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded | 
| Manufacturer | Arkema | 
| Trade Name | KYNAR® | 
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Arkema Group KYNAR® 2821-00 Polyvinylidene Fluoride Powder.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Bulk Density | 0.288 g/cc | 0.0104 lb/in³ | |
| Particle Size | 5.0 µm | 5.0 µm | Loosely agglomerated | 
| Particle Mesh Size | 14 Mesh | 14 Mesh | |
| Viscosity | 1.20e+6 - 2.00e+6           cP @Shear Rate 100 1/s, Temperature 232 °C | 1.20e+6 - 2.00e+6           cP @Shear Rate 100 1/s, Temperature 450 °F | Melt Viscosity; ASTM D3835 | 
| Melt Flow | 1.0 - 6.0           g/10 min @Load 5.00 kg, Temperature 232 °C | 1.0 - 6.0           g/10 min @Load 11.0 lb, Temperature 450 °F | ASTM D1238 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Melting Point | 140 - 145 °C | 284 - 293 °F |