Aremco Pyro-Tape™ 682-DS High Temperature Tape Double sided, single layer, fiberglass tape with silicone adhesive

Category Polymer , Adhesive , Tape
Manufacturer Aremco
Trade Name Pyro-Tape™
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Aremco Pyro-Tape™ 682-DS High Temperature Tape Double sided, single layer, fiberglass tape with silicone adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications Double Sided Features Assembly of high temp components and films.
Physical Properties Metric English Comments
Thickness 178 microns
7.00 mil
Thermal Properties Metric English Comments
Maximum Service Temperature, Air -73.0 °C
-99.4 °F
260 °C
500 °F
Descriptive Properties Value Comments
Adhesion 25 oz/in
Tape Tensile Strength 175 lbs/in