Category | Polymer , Thermoplastic , Elastomer, TPE |
Manufacturer | AlphaGary |
Trade Name | AlphaSeal™ |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | AlphaGary AlphaSeal™ 04-073 P Modified Thermoplastic Elastomer.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.890 g/cc | 0.890 g/cc |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 71 | 71 | |
Tensile Strength | 8.27 MPa | 1200 psi | |
Elongation at Break | 600 % | 600 % |