Abatron AboSeal 8104-17 Acrylic-Latex Based Sealant and Caulk; High-Density

Category Polymer , Adhesive , Thermoset
Manufacturer Abatron
Trade Name AboSeal
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboSeal 8104-17 Acrylic-Latex Based Sealant and Caulk; High-Density.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AboSeal 8104-17 is 80% solids and acrylic-latex based. It comes as one package and in most colors. It is known for its high density. It is the same as 8104-16 for low-odor, adhesion, quick drying and paintability, stability, retention of properties as no sag, but it is not as heavy-duty. It is also slightly lower in price. It's as easy to use as 8104-16 and 8104-18.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
Solids Content 80 %
80 %
Mechanical Properties Metric English Comments
Hardness, Shore A 36
36
Tensile Strength at Break 0.0483 MPa
7.00 psi
Elongation at Break 970 %
970 %
Processing Properties Metric English Comments
Extrusion Rate 54.0 g/min
54.0 g/min
Semco
Descriptive Properties Value Comments
Color Most Colors