3M Dyneon™ PFA 6502TZ Perfluoroalkoxy Fluorothermoplastic Granules

Category Polymer , Thermoplastic , Fluoropolymer , PFA
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ PFA 6502TZ Perfluoroalkoxy Fluorothermoplastic Granules.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Dyneon™ PFA 6502TZ is a fluorothermoplastic resin for transfer molding applications and extrusion of claddings and linings. Dyneon PFA 6502TZ allows for easy processing under low shear rates, with a wide processing window and excellent color stability. This material can be used in tough environments, such as chemical industry applications, where high strength and extreme thermal and chemical resistance are required.Features and Benefits:Wide service temperature rangeExcellent, almost universal resistance to solvents and chemicalsHigh transparencyExtremely high weathering resistance and UV stabilitySmooth surfacesBroad processing windowHigh limiting oxygen index: does not support combustionGood non stick characteristics Excellent electrical insulation propertiesExcellent mold release Good low friction propertiesExcellent stress crack resistanceTransfer molding and extrusionInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
ASTM D792
Melt Index of Compound 2.0 g/10 min

@Load 5.00 kg,
Temperature 372 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 380 %
380 %
ASTM D638
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 310 °C
590 °F
ASTM D4591
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Descriptive Properties Value Comments
Form Pellets