HOME
ABOUT US
PRODUCT
Thermoplastic
Thermoset
Adhesive
RenewableRecycled-Polymer
RenewableRecycled-Film
Tape
RECENT UPDATE
Company News
Product News
CONTACT US
RFQ
POLYMER SEARCH
SEARCH
HOME
POLYMER SEARCH
Plastcom spol. s r.o.
Plastcom spol. s r.o. > Polypropylene with 40% Glass Fiber Filler
Manufacturer :
Plastcom spol. s r.o.
>
Category :
Polypropylene with 40% Glass Fiber Filler
Product List
Tips:
Up to 100 items are displayed.
PRODUCT NO.
Category
Trade Name
Plastcom SLOVALEN PC 69 GF 35 FRT 4 Polypropylene Copolymer, 35% Glass Fiber, Halogen Free and Phosphor Free Flame Retardant
Polypropylene Copolymer
SLOVALEN
Plastcom SLOVALEN PH 49 GF 40 PP, 40% glass fibre
Polypropylene with 40% Glass Fiber Filler
SLOVALEN
Plastcom SLOVALEN PH 69 GF 40 Polypropylene Homopolymer, 40% Glass Fiber
Polypropylene with 40% Glass Fiber Filler
SLOVALEN
Plastcom SLOVALEN PC 69 GF 40 PP, 40% glass beads, mod. of mech. properties
Polypropylene with 40% Glass Fiber Filler
SLOVALEN
Plastcom SLOVALEN PH 69 GF 40 PP, 40% glass fibre, mod. of mech. properties
Polypropylene with 40% Glass Fiber Filler