PRODUCT NO. Category Trade Name
Plastcom SLOVASTER® B GF 10 Polybutylene Terephthalate, 10% Glass Fiber Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled SLOVASTER®
Plastcom SLOVASTER® B1 GF 10 FRX 5 PBT reinforced with 10% glass fibre, with flame retardant Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant SLOVASTER®
Plastcom SLOVASTER® B1 GF 10 PBT, 10% glass fibre Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled SLOVASTER®
Plastcom SLOVASTER® B1 GF 6 HML PBT, 6% glass fibre Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled SLOVASTER®
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled SLOVASTER®
Plastcom SLOVASTER® B2 GF 10 PBT, 10% glass fibre Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled SLOVASTER®
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled SLOVASTER®
Plastcom SLOVASTER® B1 GF 6 PBT, 6% glass fibre Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled SLOVASTER®
Plastcom SLOVASTER® B1 HML GF 10 PBT, 10% glass fibre Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled SLOVASTER®