HOME
ABOUT US
PRODUCT
Thermoplastic
Thermoset
Adhesive
RenewableRecycled-Polymer
RenewableRecycled-Film
Tape
RECENT UPDATE
Company News
Product News
CONTACT US
RFQ
POLYMER SEARCH
SEARCH
HOME
POLYMER SEARCH
Plastcom spol. s r.o.
Plastcom spol. s r.o. > Nylon 6, Glass Bead Filled
Manufacturer :
Plastcom spol. s r.o.
>
Category :
Nylon 6, Glass Bead Filled
Product List
Tips:
100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO.
Category
Trade Name
Plastcom SLOVAMID 6 GB 30 HI PA6 reinforced with glass beads, improved impact strength
Nylon 6, Glass Bead Filled
SLOVAMID
Plastcom SLOVAMID 6 GB 30 PA6, 30% glass beads
Nylon 6, Glass Bead Filled
SLOVAMID 6
Plastcom SLOVAMID 6 GF 20 GB 10 PA6, 20% glass fibre, 10% glass beads
Nylon 6, Glass Bead Filled
SLOVAMID 6
Plastcom SLOVAMID 6 GF 20 LS PA6, 20% glass beads, light stability
Nylon 6, Glass Bead Filled
SLOVAMID 6
Plastcom SLOVAMID 6 GF 20 PA6, 20% glass beads
Nylon 6, Glass Bead Filled
SLOVAMID 6
Plastcom SLOVAMID 6 GB 30 TS PA6, 30% glass beads
Nylon 6, Glass Bead Filled
SLOVAMID 6
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre, 20% glass beads
Nylon 6, Glass Bead Filled
SLOVAMID 6
Plastcom SLOVAMID 6 GB 20 PA6 reinforced with 20% glass beads