Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong) > Category : Polycarbonate, Unreinforced, Flame Retardant Product List

Tips:100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Category Trade Name
Cheng Yu Plastic ML848 Flame Retardant PC Polycarbonate, Unreinforced, Flame Retardant
Cheng Yu Plastic ML849 Flame Retardant PC Polycarbonate, Unreinforced, Flame Retardant