Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : CP-Polymer-Technik GmbH & Co. > Category : Nylon 66, Glass/Mineral Filled Product List

Tips:100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Category Trade Name
CP-Polymer-Technik Wellamid® 6600 MRGV 20/20 HWCP 20% Mineral and 20% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Nylon 66, Glass/Mineral Filled Wellamid®
CP-Polymer-Technik Wellamid® 6600 MRGV 20/20 HWCP 20% Mineral and 20% Glass Fiber Nylon 66, Heat Stabilized, Dry Nylon 66, Glass/Mineral Filled Wellamid®
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Nylon 66, Glass/Mineral Filled Wellamid®
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Dry Nylon 66, Glass/Mineral Filled Wellamid®