Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : ATI Allvac > Category : Maraging Steel Product List

Tips:100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Category Trade Name
ATI Allvac® Vasco® 9-4-30 Specialty Steel, Heat Treatment: 899°C (1650°F) + Age Maraging Steel Vasco®
ATI Allvac® VascoMax® C-250 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age Maraging Steel VascoMax®
ATI Allvac® VascoMax® C-300 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age Maraging Steel VascoMax®
ATI Allvac® VascoMax® C-350 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age Maraging Steel VascoMax®
ATI Allvac® VascoMax® T-250 Specialty Steel, Heat Treatment: 816°C (1500°F) + Age Maraging Steel VascoMax®