Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 575 V @Temperature 23.0 °C |
575 V @Temperature 73.4 °F |
DAM; IEC 60112 |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 575 V @Temperature 23.0 °C |
575 V @Temperature 73.4 °F |
DAM; UL 746A |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |