Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim.. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim.. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid A G10 FR PH1 50% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G10 FR PH1 was developed specifically for highly loaded, structural applications in the electrical industry. It combines extremely high mechanical performance with flame retar.. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid A G10 FR PH1 50% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G10 FR PH1 was developed specifically for highly loaded, structural applications in the electrical industry. It combines extremely high mechanical performance with flame retar.. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6 Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex.. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid B G4 FR HF 20% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G4 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid B G4 FR HF 20% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G4 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid B G6 FR HF 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid B G6 FR HF 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6 Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au.. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,.. |
|||
Comparative Tracking Index | 550 V @Thickness 3.20 mm |
550 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu.. |
|||
Comparative Tracking Index | >= 550 V @Temperature 23.0 °C |
>= 550 V @Temperature 73.4 °F |
DAM; UL 746A |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |