Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 23.0 °C |
1.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 23.0 °C |
1.00e+14 ohm-cm @Temperature 73.4 °F |
DAM; ASTM D257 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm @Temperature 25.0 °C |
>= 1.00e+14 ohm-cm @Temperature 77.0 °F |
|
Master Bond EP112LS Two part, heat curing epoxy for potting, encapsulation, coating, sealing and impregnation Master Bond EP112LS is a low viscosity two component epoxy resin system for potting, encapsulation, sealing, coating and impregnation. The mix ratio is an easy to use 100:80 by weight. EP112LS offer.. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm @Temperature 25.0 °C |
>= 1.00e+14 ohm-cm @Temperature 77.0 °F |
ASTM-D257 |
CeramTec 665 Steatite, MgO•SiO2 Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. 665 L533C has low dielectric loss. It makes exc.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 25.0 °C |
1.00e+14 ohm-cm @Temperature 77.0 °F |
ASTM-D257 |
CeramTec 701 Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 20.0 °C |
1.00e+14 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec B 601 Alumina, 98.5% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 20.0 °C |
1.00e+14 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2 DN 70 is a ZTA Alumina Toughened Zirconia. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm @Temperature 20.0 °C |
>= 1.00e+14 ohm-cm @Temperature 68.0 °F |
|
CeramTec Rubalit® A 1894 Alumina, 94% Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 20.0 °C |
1.00e+14 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec V 679 Alumina, 99.7% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm @Temperature 25.0 °C |
>= 1.00e+14 ohm-cm @Temperature 77.0 °F |
ASTM-D1829 |
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm @Temperature 25.0 °C |
>= 1.00e+14 ohm-cm @Temperature 77.0 °F |
ASTM-D1829 |
CoorsTek ADS-96R 96% Alumina Thick Film Substrate This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm @Temperature 25.0 °C |
>= 1.00e+14 ohm-cm @Temperature 77.0 °F |
ASTM-D257 |
CoorsTek ADS-995 99.5% Alumina Thin Film Applications: thin film substrates |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm @Temperature 25.0 °C |
>= 1.00e+14 ohm-cm @Temperature 77.0 °F |
ASTM-D257 |
CoorsTek ADS-996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm @Temperature 25.0 °C |
>= 1.00e+14 ohm-cm @Temperature 77.0 °F |
ASTM-D1829 |
CoorsTek PlasmaPure-UC™ 99.9% Alumina |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm @Temperature 100 °C |
>= 1.00e+14 ohm-cm @Temperature 212 °F |
ASTM-D257 |
CoorsTek Superstrate® 996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm @Temperature 300 °C |
>= 1.00e+14 ohm-cm @Temperature 572 °F |
ASTM-D257 |
CoorsTek Superstrate® TPS 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 20.0 °C |
1.00e+14 ohm-cm @Temperature 68.0 °F |
|
Anderman Ceramics EA95 Sintered Alumina, 95% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 20.0 °C |
1.00e+14 ohm-cm @Temperature 68.0 °F |
|
Anderman Ceramics EA96 Sintered Alumina, 96% High strength alumina (96%) available pink or white. Available in many shapes and sizes.Information provided by Anderman Ceramics. |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 20.0 °C |
1.00e+14 ohm-cm @Temperature 68.0 °F |
|
Anderman Ceramics EA995 Sintered Alumina, 99.5% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 20.0 °C |
1.00e+14 ohm-cm @Temperature 68.0 °F |
|
Anderman Ceramics EAZ 20 Zirconia Toughened Alumina Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 20.0 °C |
1.00e+14 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec B 40 Alumina, 99.1% B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm @Temperature 20.0 °C |
>= 1.00e+14 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec Rubalit® A 1896 Alumina Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele.. |