Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.40e+14 ohm-cm @Temperature 20.0 °C |
5.40e+14 ohm-cm @Temperature 68.0 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Volume Resistivity | 5.40e+14 ohm-cm @Temperature 90.0 °C |
5.40e+14 ohm-cm @Temperature 194 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Volume Resistivity | 5.40e+14 ohm-cm @Temperature 90.0 °C |
5.40e+14 ohm-cm @Temperature 194 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Volume Resistivity | 5.40e+14 ohm-cm @Temperature 90.0 °C |
5.40e+14 ohm-cm @Temperature 194 °F |
ASTM D257 |
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Volume Resistivity | 5.40e+14 ohm-cm @Temperature 90.0 °C |
5.40e+14 ohm-cm @Temperature 194 °F |
ASTM D257 |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |