Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.60e+7 ohm-cm @Temperature 250 °C |
1.60e+7 ohm-cm @Temperature 482 °F |
|
Schott Glass 8625 Biocompatible Glass Biocompatible glass, high IR-absorbing, Transponders (implantable) The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by S.. |
|||
Volume Resistivity | 1.60e+7 ohm-cm @Temperature 250 °C |
1.60e+7 ohm-cm @Temperature 482 °F |
DIN 52326 |
Schott Nextrema® 712-6 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |