Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.30e+15 ohm-cm @Temperature 20.0 °C |
1.30e+15 ohm-cm @Temperature 68.0 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Volume Resistivity | 1.30e+15 ohm-cm @Temperature 20.0 °C |
1.30e+15 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Volume Resistivity | 1.30e+15 ohm-cm @Temperature 90.0 °C |
1.30e+15 ohm-cm @Temperature 194 °F |
ASTM D257 |
Solvay Specialty Polymers Polidiemme® G/420 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Si.. |