Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 275 °C |
1.00e+9 ohm-cm @Temperature 527 °F |
Result based on 450G |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 275 °C |
1.00e+9 ohm-cm @Temperature 527 °F |
IEC 60093 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 275 °C |
1.00e+9 ohm-cm @Temperature 527 °F |
IEC 60093 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 275 °C |
1.00e+9 ohm-cm @Temperature 527 °F |
IEC 60093 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 275 °C |
1.00e+9 ohm-cm @Temperature 527 °F |
IEC 60093 |
Victrex® PEEK 90G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 275 °C |
1.00e+9 ohm-cm @Temperature 527 °F |
IEC 60093 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 250 °C |
1.00e+9 ohm-cm @Temperature 482 °F |
|
Schott Glass 8688 Borosilicate Glass Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 400 °C |
1.00e+9 ohm-cm @Temperature 752 °F |
ASTM-D1829 |
CeramTec Rubalit® 600 Alumina, 48% Rubalit® 600 is suitable for both mechanical and laser trimming and is chiefly used as the core for high-grade carbon-film resistors. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 900 °C |
1.00e+9 ohm-cm @Temperature 1650 °F |
|
CeramTec Rubalit® 710 Alumina, 99.6% Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conduct.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 500 °C |
1.00e+9 ohm-cm @Temperature 932 °F |
ASTM-D1829 |
CoorsTek ADS-96R 96% Alumina Thick Film Substrate This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers |
|||
Volume Resistivity | >= 1.00e+9 ohm-cm @Temperature 500 °C |
>= 1.00e+9 ohm-cm @Temperature 932 °F |
ASTM-D257 |
CoorsTek ADS-995 99.5% Alumina Thin Film Applications: thin film substrates |
|||
Volume Resistivity | >= 1.00e+9 ohm-cm @Temperature 300 °C |
>= 1.00e+9 ohm-cm @Temperature 572 °F |
ASTM-D1829 |
CoorsTek ADS-995R MidFilm™ 99.5% Alumina Thick Film Applications: thick films and lasers |
|||
Volume Resistivity | >= 1.00e+9 ohm-cm @Temperature 500 °C |
>= 1.00e+9 ohm-cm @Temperature 932 °F |
ASTM-D257 |
CoorsTek ADS-996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Volume Resistivity | >= 1.00e+9 ohm-cm @Temperature 700 °C |
>= 1.00e+9 ohm-cm @Temperature 1290 °F |
ASTM-D257 |
CoorsTek Superstrate® 996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Volume Resistivity | <= 1.00e+9 ohm-cm @Temperature 93.0 °C |
<= 1.00e+9 ohm-cm @Temperature 199 °F |
|
Abatron AboCast 7703-21/AboCure 7703-23 (C) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Volume Resistivity | <= 1.00e+9 ohm-cm @Temperature 93.0 °C |
<= 1.00e+9 ohm-cm @Temperature 199 °F |
|
Abatron AboCast 7703-21/AboCure 7703-24 (D) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Volume Resistivity | <= 1.00e+9 ohm-cm @Temperature 66.0 °C |
<= 1.00e+9 ohm-cm @Temperature 151 °F |
|
Abatron AboCast 7703-21/AboCure 7703-25 (E) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Volume Resistivity | <= 1.00e+9 ohm-cm @Temperature 93.0 °C |
<= 1.00e+9 ohm-cm @Temperature 199 °F |
|
Abatron AboCast 7703-21/AboCure 7703-25 (E) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 600 °C |
1.00e+9 ohm-cm @Temperature 1110 °F |
|
Anderman Ceramics EAZ 20 Zirconia Toughened Alumina Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 275 °C |
1.00e+9 ohm-cm @Temperature 527 °F |
Results based on HT G22 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 275 °C |
1.00e+9 ohm-cm @Temperature 527 °F |
|
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 275 °C |
1.00e+9 ohm-cm @Temperature 527 °F |
IEC 60093 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm @Temperature 275 °C |
1.00e+9 ohm-cm @Temperature 527 °F |
IEC 60093 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |