Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 23.0 °C |
1.00e+11 ohm-cm @Temperature 73.4 °F |
50%RH; IEC 60093 |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 23.0 °C |
1.00e+11 ohm-cm @Temperature 73.4 °F |
50%RH; ASTM D257 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 23.0 °C |
1.00e+11 ohm-cm @Temperature 73.4 °F |
50%RH; IEC 60093 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm @Temperature 150 °C |
>= 1.00e+11 ohm-cm @Temperature 302 °F |
DC; DIN 40634 or VDE 0345 |
Mitsubishi Hostaphan® RN, 36 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 350 °C |
1.00e+11 ohm-cm @Temperature 662 °F |
|
Schott Glass 8240 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, free from alkali, blue colored, defined absorption Bulb and exhaust tube .. |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 350 °C |
1.00e+11 ohm-cm @Temperature 662 °F |
|
Schott Glass 8253 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, for use at higher temperatures than glass 8252, free from alkali Bulb and.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 250 °C |
1.00e+11 ohm-cm @Temperature 482 °F |
|
Schott Glass 8531 Soft Glass Soft glass, free from Na, of high lead content, high dielectric constant Encapsulation of semiconductor components at low temperature (diodes)Information provided by SCHOTT AG. |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 250 °C |
1.00e+11 ohm-cm @Temperature 482 °F |
|
Schott Glass 8532 Soft Glass Soft glass, free from Na, of high lead content, lower sealing temperature than glass 8531, high dielectric constant Encapsulation of semiconductor components at low temperature (diodes)Information .. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm @Temperature 70.0 °C |
>= 1.00e+11 ohm-cm @Temperature 158 °F |
|
Sibur 140-13A Compound 8/2 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm @Temperature 70.0 °C |
>= 1.00e+11 ohm-cm @Temperature 158 °F |
|
Sibur 140-13P Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 200 °C |
1.00e+11 ohm-cm @Temperature 392 °F |
ASTM-D257 |
CeramTec Rubalit® 600 Alumina, 48% Rubalit® 600 is suitable for both mechanical and laser trimming and is chiefly used as the core for high-grade carbon-film resistors. |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 400 °C |
1.00e+11 ohm-cm @Temperature 752 °F |
ASTM-D1829 |
CeramTec Rubalit® 708 Alumina, 96% Based on 96% aluminum oxide, Rubalit® 708 was developed specifically for making heavy-duty resistors and miniature metal layer resistors. Because of its outstanding strength, this same material is .. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm @Temperature 400 °C |
>= 1.00e+11 ohm-cm @Temperature 752 °F |
|
CeramTec Rubalit® A 1894 Alumina, 94% Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm @Temperature 400 °C |
>= 1.00e+11 ohm-cm @Temperature 752 °F |
IEC 672-1 |
CeramTec Rubalit® IS 95 Alumina Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 400 °C |
1.00e+11 ohm-cm @Temperature 752 °F |
ASTM-D257 |
CeramTec CeramCool® Rubalit® 708 Alumina, 96% CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 400 °C |
1.00e+11 ohm-cm @Temperature 752 °F |
IEC 345 |
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance) Rubalit® 708 HP (High Performance) has been developed from Rubalit® 708S. This material shares the same chemical composition, is produced on the same plant and using the identical production techn.. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm @Temperature 400 °C |
>= 1.00e+11 ohm-cm @Temperature 752 °F |
IEC 672-1 |
CeramTec Rubalit® A 1896 Alumina Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 350 °C |
1.00e+11 ohm-cm @Temperature 662 °F |
|
Schott Glass 8241 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, free from alkali, blue colored, defined absorption Bulb and exhaust tube .. |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 23.0 °C |
1.00e+11 ohm-cm @Temperature 73.4 °F |
50%RH; IEC 60093 |
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) Zytel® 70G35HSLX BK357 is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm @Temperature 400 °C |
>= 1.00e+11 ohm-cm @Temperature 752 °F |
|
CeramTec Rubalit® A 1898 Alumina, 98% Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |