Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+10 ohm-cm @Temperature 250 °C |
1.00e+10 ohm-cm @Temperature 482 °F |
|
Schott Glass 8250 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, low refractive index, good insulator X-ray tubes, transmitting tubes, image amplifier tubes, He-Ne-lase.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Temperature 350 °C |
1.00e+10 ohm-cm @Temperature 662 °F |
|
Schott Glass 8651 Sealing Glass Tungsten sealing glass Power diodesInformation provided by SCHOTT AG. |
|||
Volume Resistivity | >= 1.00e+10 ohm-cm @Temperature 150 °C |
>= 1.00e+10 ohm-cm @Temperature 302 °F |
|
Master Bond EP112LS Two part, heat curing epoxy for potting, encapsulation, coating, sealing and impregnation Master Bond EP112LS is a low viscosity two component epoxy resin system for potting, encapsulation, sealing, coating and impregnation. The mix ratio is an easy to use 100:80 by weight. EP112LS offer.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Temperature 400 °C |
1.00e+10 ohm-cm @Temperature 752 °F |
IEC 672-1 |
CeramTec B 601 Alumina, 98.5% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Temperature 400 °C |
1.00e+10 ohm-cm @Temperature 752 °F |
ASTM-D1829 |
CeramTec Rubalit® 702 Alumina, 85% Rubalit® 702 is a high-performance material for the manufacturing of metal-film resistors. With an alumina content of 85%, it provides extreme hardness and high thermal conductivity. Practical appl.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Temperature 20.0 °C |
1.00e+10 ohm-cm @Temperature 68.0 °F |
IEC 345 |
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate) Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Temperature 200 °C |
1.00e+10 ohm-cm @Temperature 392 °F |
IEC 345 |
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate) Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Temperature 20.0 °C |
1.00e+10 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec SL 303 Silicon Nitride, SiAION+SiC SL 303 is a silicon nitride ceramic. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile i.. |
|||
Volume Resistivity | >= 1.00e+10 ohm-cm @Temperature 500 °C |
>= 1.00e+10 ohm-cm @Temperature 932 °F |
ASTM-D257 |
CoorsTek Superstrate® 996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Volume Resistivity | >= 1.00e+10 ohm-cm @Temperature 700 °C |
>= 1.00e+10 ohm-cm @Temperature 1290 °F |
ASTM-D257 |
CoorsTek Superstrate® TPS 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm @Temperature 1000 °C |
1.00e+10 - 1.00e+12 ohm-cm @Temperature 1830 °F |
|
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain) LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good .. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Temperature 130 °C |
1.00e+10 ohm-cm @Temperature 266 °F |
ASTM D257 |
3M Scotchcast™ 265 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 265 is a new solution to an old problem. Historically, manufactures of coils, stators and armatures have used liquid-based varnishes or resins to coat and impregnate t.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Temperature 400 °C |
1.00e+10 ohm-cm @Temperature 752 °F |
IEC 672-1 |
CeramTec B 40 Alumina, 99.1% B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Temperature 600 °C |
1.00e+10 ohm-cm @Temperature 1110 °F |
ASTM-D257 |
CeramTec CeramCool® Rubalit® 708 Alumina, 96% CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |