Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.50e+16 - 4.15e+16 ohm-cm | 2.50e+16 - 4.15e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Volume Resistivity | 2.50e+16 - 4.15e+16 ohm-cm | 2.50e+16 - 4.15e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Asia Pacific) Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Volume Resistivity | 2.50e+16 - 4.15e+16 ohm-cm | 2.50e+16 - 4.15e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |