Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7000 ohm-cm | 7000 ohm-cm | Approximate value obtained from graphical representation; CTM E043 |
Nanocyl PLASTICYL™ PBT1501 Polybutylene Terephthalate with 3 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |