Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 50000 ohm-cm | 50000 ohm-cm | IEC 60093 |
SABIC Innovative Plastics LNP Faradex DX07304 PC (Asia Pacific) CF filled grade with EMI shieldingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Volume Resistivity | 50000 ohm-cm | 50000 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC3508 PPE+HIPS (Europe-Africa-Middle East) PRELIMINARY DATA. LNP* Stat-kon* Noryl_NC3508 compound is a 33% glass/mineral/carbon filled PPE+PS. ESD, high heat, tight tolerance: electronic packaging/chip trays. |
|||
Volume Resistivity | 50000 ohm-cm | 50000 ohm-cm | |
LATI Latamid 66 H2 K/20 PA 66, 20% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |