Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 50 ohm-cm | 50 ohm-cm | |
LATI Latamid 66 H2 K/50 PA 66, 50% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Volume Resistivity | 50 ohm-cm | 50 ohm-cm | ASTM D257 |
Techmer ES Electrablend® POM Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveTPCI# 9961114Information provided by TP Composites, Inc. |
|||
Volume Resistivity | 50 ohm-cm | 50 ohm-cm | ASTM D257 |
Techmer ES Statiblend® HDPE C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveUL File Number: E157318Appearance: BlackTPCI# 9411115Information provided by TP Composites.. |
|||
Volume Resistivity | 50 - 100 ohm-cm | 50 - 100 ohm-cm | |
Master Bond MasterSil 705C Non-Corrosive Silicone with Carbon Filler Description: Master Bond MasterSil 705C is an electrically conductive, one component, non-corrosive, carbon filled silicone for bonding, sealing and coating. This black colored paste like system cur.. |
|||
Volume Resistivity | 50 ohm-cm @Time 300 sec |
50 ohm-cm @Time 0.0833 hour |
18% Carbon Black |
TIMCAL ENSACO™ 260G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Volume Resistivity | <= 50 ohm-cm | <= 50 ohm-cm | IEC 93 |
CP-Polymer-Technik Wellamid® 6600 CF10 HWCP 10% Carbon Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Volume Resistivity | 50 ohm-cm | 50 ohm-cm | ASTM D257 |
Techmer ES Statiblend® PP CO 99074 Availability: North AmericaForms: PelletsFeature: Copolymer and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Volume Resistivity | <= 50 ohm-cm | <= 50 ohm-cm | IEC 93 |
CP-Polymer-Technik Wellamid® 6000 CF 10 HWCP 10% Carbon Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Volume Resistivity | <= 50 ohm-cm | <= 50 ohm-cm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® PA 1411 Conductive Thermoplastic Compound PRE-ELEC® PA 1411 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. PRE-ELEC® PA 1411 has a very low electrical resistivity. P.. |
|||
Volume Resistivity | 50 ohm-cm | 50 ohm-cm | ASTM D257 |
PolyOne Edgetek® PF-40CF/000 Polysulfone, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 50 ohm-cm | 50 ohm-cm | IEC 60093 |
Polyplastics Duracon® EB-10 Acetal Co-polymer (POM), Conductive, Antistatic DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |