Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.00e+12 ohm-cm | 5.00e+12 ohm-cm | |
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Clear is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to .. |
|||
Volume Resistivity | 5.00e+12 ohm-cm | 5.00e+12 ohm-cm | Condition A; IPC 2.5.17.1 |
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowLow Z-axis expansion. Provides reliable plated through holes in multi-layer boardsTight .. |
|||
Volume Resistivity | 5.00e+12 ohm-cm | 5.00e+12 ohm-cm | |
Pyrotek TS-111 Thermoset Electrical Insulation Product (Nema Grade: G-11) Glass reinforcement, Epoxy Resin, Natural Color. Good electrical and mechanical properties.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators M.. |
|||
Volume Resistivity | 5.00e+12 ohm-cm | 5.00e+12 ohm-cm | Conditioned; IEC 60093 |
Lanxess Durethan® DP AKV 30 FN00 000000 Nylon 66, 30% Glass Fiber PA 66, injection molding 30% glass fibers, UL 94 V-0 at 0.4 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, free from halogen and red phosphorous |
|||
Volume Resistivity | 5.00e+12 ohm-cm | 5.00e+12 ohm-cm | cond.; IEC 60093 |
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Volume Resistivity | >= 5.00e+12 ohm-cm @Temperature 70.0 °C |
>= 5.00e+12 ohm-cm @Temperature 158 °F |
|
Sibur Neva Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Volume Resistivity | >= 5.00e+12 ohm-cm | >= 5.00e+12 ohm-cm | |
Epoxy Technology EPO-TEK® T7109-19 Electrically Insulating Epoxy Paste Material Description: A flexible, thermally conductive, electrically insulating epoxy paste designed for low stress and heat dissipation applications. It is an alternative to EPO-TEK® T7109-17, de.. |
|||
Volume Resistivity | 5.00e+12 ohm-cm | 5.00e+12 ohm-cm | |
Covestro Texin® 270 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Volume Resistivity | 5.00e+12 ohm-cm | 5.00e+12 ohm-cm | |
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e.. |
|||
Volume Resistivity | 5.00e+12 ohm-cm | 5.00e+12 ohm-cm | ASTM D257 |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Volume Resistivity | >= 5.00e+12 ohm-cm | >= 5.00e+12 ohm-cm | |
CEN® Electronic Material CN Polyimide Film, 7 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Volume Resistivity | >= 5.00e+12 ohm-cm | >= 5.00e+12 ohm-cm | ASTM D257 |
CEN® Electronic Material CV Polyimide Film, 6 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |
|||
Volume Resistivity | 5.00e+12 ohm-cm | 5.00e+12 ohm-cm | |
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m.. |
|||
Volume Resistivity | >= 5.00e+12 ohm-cm | >= 5.00e+12 ohm-cm | |
CEN® Electronic Material CN Polyimide Film, 6 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Volume Resistivity | >= 5.00e+12 ohm-cm | >= 5.00e+12 ohm-cm | ASTM D257 |
CEN® Electronic Material CV Polyimide Film, 7 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |
|||
Volume Resistivity | 5.00e+12 ohm-cm | 5.00e+12 ohm-cm | ASTM D257 |
PolyOne Geon™ Vinyl Wire & Cable W9200 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |