Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.40e+14 ohm-cm | 4.40e+14 ohm-cm | |
Momentive Performance Materials RTV8262 Silicone Rubber Compounds for Potting, Encapsulating and Sealing RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr.. |
|||
Volume Resistivity | 4.40e+14 ohm-cm | 4.40e+14 ohm-cm | |
Momentive Performance Materials RTV60 Silicone Rubber Compound for High Temperature, Red RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa.. |
|||
Volume Resistivity | 4.40e+14 ohm-cm | 4.40e+14 ohm-cm | ASTM D247 |
Plenco 1500 Polyester, Granular, Compression Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |