Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Rogers Corporation TMM® TMM3 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | 96 hours at 90°C; 50% RH; ASTM D257 |
PTS Tristar® PC-10FR-(VIK) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Impact Modifier and Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV102 One Component Acetoxy Adhesive Sealant, White RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV103 One Component Acetoxy Adhesive Sealant, Black RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | IEC 60093 |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV108 One Component Acetoxy Adhesive Sealant, Translucent RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV109 One Component Acetoxy Adhesive Sealant, Aluminum RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV133 Black, Flame Retardant, One Component Silicone Sealant RTV 133 black, one-component, ready-to-use rubber adhesive sealant is recommended for evaluation in applications in the electronic, aerospace, appliance, transportation and other industries where re.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV5242 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV5243 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV5249 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | IEC 60093 |
Lanxess Durethan® DP 2131/20 W1 901317 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, weather resistance, good heat-ageing resistance |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF33 HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: Lubricated and Heat StabilizedProcessi.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF35 HS L 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: Lubricated and Heat StabilizedProcessi.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT 1226 Availability: North AmericaForms: PelletsFeatures: Medium FlowAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT 613 Availability: North AmericaForms: PelletsFeatures: Good Flow and Good ProcessabilityAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT E Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Extrusion and Injection MoldingInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT WM35 X Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT 0143 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT 0150 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT 0158 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | IEC 60093 |
Polyplastics Duranex® 7407 Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Loctite® 3534 Glob Top Encapsulant COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Dow Corning SE 4402 KIT One-part, grey, heat cure, good flowability, thermally conductive, controlled volatility.Information provided by Dow Corning |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Dow Corning SE 738 SILICONE RTV One-part, white, moisture cure RTV, non-flowing, general purpose, UL 94 HB.Information provided by Dow Corning |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | IEC 60093 |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Aremco Aremco-Bond™ 2318 High Performance Epoxide |