Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.90e+15 ohm-cm @Temperature 23.0 °C |
2.90e+15 ohm-cm @Temperature 73.4 °F |
50% RH, ASTM D257-07; ASTM D257 |
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
Volume Resistivity | 2.90e+15 ohm-cm @Temperature 23.0 °C |
2.90e+15 ohm-cm @Temperature 73.4 °F |
50%RH, ASTM D257-07; ASTM D257 |
PolyOne OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 315-01 a is non-halogen flame retardant material designed for flexible power cord insulation, cable jackets, and ribbon cables. New Product. Commercial specifications have not been est.. |
|||
Volume Resistivity | 2.90e+15 ohm-cm @Temperature 23.0 °C |
2.90e+15 ohm-cm @Temperature 73.4 °F |
50% RH, ASTM D257-07; ASTM D257 |
PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 320-01 is a non-halogen flame retardant material designed for flexible power cord insulation and cable jackets. New Product. Commercial specifications have not been established. - Non-.. |
|||
Volume Resistivity | 2.90e+15 ohm-cm | 2.90e+15 ohm-cm | ASTM D257 |
PolyOne Geon™ Vinyl Flexible R3792E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Volume Resistivity | 2.90e+15 ohm-cm | 2.90e+15 ohm-cm | ASTM D257 |
Ensinger Tecatron® XP-64 Compression Molded PPS Compound, 40% Fiberglass Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |