Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.90e+11 ohm-cm | 2.90e+11 ohm-cm | |
Saint-Gobain Korel® K20 Very Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Volume Resistivity | 2.90e+11 ohm-cm | 2.90e+11 ohm-cm | ASTM D247 |
Plenco 4301 Phenolic, Granular, Compression Molded PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava.. |