Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Lexan® PPC4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | >= 2.60e+17 ohm-cm | >= 2.60e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |