Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | Conditioned; ASTM D257 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | Conditioned; ASTM D257 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
LG Chemical LUPOY GN1006FL PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
LG Chemical LUPOY GP1000L PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | |
Momentive Performance Materials TSE326 High Temperature, Heat Cured One Component Silicone Adhesive TSE326 is a one-component, heat curing silicone adhesive which offers extended performance at temperatures exceeding 200C. A flowable material with primerless adhesion to many substrates, it is suit.. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | |
Momentive Performance Materials TSE399 One Component RTV Adhesive Sealant/Coating, Clear/White/Black TSE392, TSE397 and TSE399 adhesive sealants/coatings are one component RTV’s that cure quickly by reacting with atmospheric moisture forming a soft dielectric silicone rubber. These materials i.. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
LG Chemical LUPOY GP1000MD PC, Light Diffusion Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
LG Chemical LUPOY GP1000MU PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: IT/OA Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provided by LG C.. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
LG Chemical LUPOY GP1000SW PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: Keypad for Mobile Phone, Automotive (Interior)CAS: 103598-77-2Information provided by LG Chemical |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL WCD933 PPE-TPE Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN.. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | IEC 60093 |
Polyplastics Duranex® 6370B Polybutylene Terephthalate (PBT), Anisotropy improvement, 30% GB filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | IEC 60093 |
Polyplastics FR-PET® C9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | |
Dow Corning SILASTIC® 9220/55 KIT PARTS A&B 55 Durometer, 2-part, 1 to 1 mix, black Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | DIN 53 482, VDE 0303, Part 3 |
Hippe PAI Polyamide-imide Particularly used where high strength in a wide range of temperature (-190°C…+260°C), high notched strength and very good dielectric properties are required. Features good chemical stability, fl.. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | |
Dow Corning 1890 PROTECTIVE COATING Silicone RTV in solvent dispersionInformation provided by Dow Corning |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
Fainplast Compounds Hax™ HF 045/16M Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, low shrinkageInformation provided by Fainplast Compounds |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | IEC 60093 |
Barlog Plastics KEBAFORM C 274 VT POM Copolymer unreinforced, antistatic POMInformation provided by BARLOG plastics GmbH. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | IEC 93 |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | |
Aremco Aremco-Bond™ 2220 High Performance Epoxide Ceramic-Filled, High Chemical Resistance, Machinable. For Repairing Deeply-Corroded Parts. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | 50% RH; ASTM D-257 |
Axiall 19940 Wire & Cable Flexible PVC 105°C rated insulation compound for 600V, 1/64 wall (18 AWG and larger) and 1000V applications. Approved by UL for THWN-2 (8 AWG and larger) and THW-2 in all sizes and colors. UL approved for 94 .. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | |
Aremco Aremco-Bond™ 2330 High Performance Epoxide Single-Part, Heat Curable, Silicone Elastomer Adhesive |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
Fainplast Compounds Hax™ HF 223F Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:High flexibility, good stress crack resistanceInformation provided by Fainplast Compound.. |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | Conditioned; ASTM D257 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | |
Chesterton 860 Moldable Polymer Gasketing Description: Chesterton® 860 Moldable Polymer Gasketing is a solid flexible gasketing material which fills in surface irregularities, stop leaks and never sticks to surfaces after curing. It is the.. |