Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 10000 ohm-cm | <= 10000 ohm-cm | 400 um thick sheet; ISO D-257 |
Premix Thermoplastics PRE-ELEC® PE 1291 PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® PE 1295 PRE-ELEC PE 1295 is a dissipative thermoplastic compound based on PE-HD. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resistance bet.. |
|||
Volume Resistivity | 10000 ohm-cm | 10000 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Volume Resistivity | <= 10000 ohm-cm | <= 10000 ohm-cm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® PE 1270
(discontinued **) PRE-ELEC PE 1270 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 12.. |
|||
Volume Resistivity | >= 10000 ohm-cm | >= 10000 ohm-cm | VDE 0303 |
GEHR Plastics PVDF-ELS Polyvinylidene Fluoride, Electrically Conductive Polyvinylidene fluoride shows a higher tensile strength, pressure resistance and dimensional stability than the related PTFE, but friction and insulation properties are lower. PVDF has a high mechan.. |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS 03008 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 10000 ohm-cm | 10000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC SS10 FR BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr.. |
|||
Volume Resistivity | 10000 - 1.00e+7 ohm-cm | 10000 - 1.00e+7 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6 GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by Weight/Unspecified Filler/Reinfor.Additive: LubricantFeatures: Conductive and LubricatedAppear.. |
|||
Volume Resistivity | 10000 ohm-cm | 10000 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA4/6 GF25 HS NAT 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Volume Resistivity | 10000 ohm-cm - 1e+05 | 10000 ohm-cm - 1e+05 | Dry; ASTM D257 |
Westlake Plastics Tempalux® CN-F Polyetherimide (conductive) Non-sloughing carbon-fiber filled material which is extremely strong and stiff, has excellent dimensional stability, and high temperature resistance to 415F. This material has broad chemical resist.. |
|||
Volume Resistivity | 10000 ohm-cm | 10000 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® L 25 NZ ESD PA12 Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of .. |
|||
Volume Resistivity | 10000 ohm-cm | 10000 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® LC-3H black PA12-CF30 Product description: Grilamid LC-3H BLACK is a Polyamide 12 injection molding product reinforced with 30 % carbon fibers. The product is inherently black and is only available in this color.Main Att.. |
|||
Volume Resistivity | 10000 ohm-cm | 10000 ohm-cm | IEC 60093 |
Eurotec® Tecomid® NA40 CR20 BK111 PA6.6, 20% carbon fiber reinforced, black Information provided by Eurotec® |
|||
Volume Resistivity | 10000 ohm-cm | 10000 ohm-cm | ASTM D257 |
Adamas Adalon® 826 PTFE, 50% Stainless steel Information provided by Adamas, HPM |