Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.80e+16 ohm-cm | 1.80e+16 ohm-cm | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 15GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Volume Resistivity | 1.80e+16 ohm-cm | 1.80e+16 ohm-cm | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 15GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Volume Resistivity | 1.80e+16 ohm-cm | 1.80e+16 ohm-cm | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 20GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Volume Resistivity | 1.80e+16 ohm-cm | 1.80e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 865 PBT+PET 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
Volume Resistivity | 1.80e+16 ohm-cm | 1.80e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific) 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
Volume Resistivity | 1.80e+16 ohm-cm | 1.80e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications. |
|||
Volume Resistivity | 1.80e+16 ohm-cm | 1.80e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL N190X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications. |
|||
Volume Resistivity | 1.80e+16 ohm-cm | 1.80e+16 ohm-cm | GB/T1410-2006 |
Sichuan Deyang Haton® hMR60DL Polyphenylene Sulfide, Glass & Mineral Reinforced Injection molding, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Volume Resistivity | 1.80e+16 ohm-cm | 1.80e+16 ohm-cm | ASTM D-257 |
UBE UPIMOL® R Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |
|||
Volume Resistivity | 1.80e+16 ohm-cm @Temperature 23.0 °C |
1.80e+16 ohm-cm @Temperature 73.4 °F |
IEC 60093 |
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |