Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.40e+17 ohm-cm | 1.40e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific) NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C |
|||
Volume Resistivity | 1.40e+17 ohm-cm | 1.40e+17 ohm-cm | 50% RH; ASTM D257 |
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating Parylene N, poly(para-xylylene), is a completely linear, highly crystalline material. Parylene N is a primary dielectric, exhibiting a very low dissipation factor, high dielectric strength, and a lo.. |
|||
Volume Resistivity | 1.40e+17 ohm-cm | 1.40e+17 ohm-cm | ASTM D257 |
DuPont™ Nomex® N196 Paper, 7 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |