Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.30e+12 ohm-cm | 1.30e+12 ohm-cm | ASTM D247 |
Plenco 00757 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |
|||
Volume Resistivity | 1.30e+12 ohm-cm | 1.30e+12 ohm-cm | |
Tra-Con Tra-Bond 77-1S One Component SMD Adhesive TRA-BOND 77-1S one component, solvent-free, insulating epoxy adhesive is designed specifically for attaching surface mounted devices (SMDs) to printed circuit boards prior to wave solder. TRA-BOND 7.. |
|||
Volume Resistivity | 1.30e+12 ohm-cm | 1.30e+12 ohm-cm | ASTM D247 |
Plenco 7552 Phenolic, Nodular, Transfer Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |
|||
Volume Resistivity | 1.30e+12 ohm-cm | 1.30e+12 ohm-cm | |
Saint-Gobain Korel® K60 Firm Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |