Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.20e+17 ohm-cm | 1.20e+17 ohm-cm | 50% RH; ASTM D257 |
Specialty Coating Systems Parylene D Poly (P-Xylylene) Coating Parylene D is a polymer of para-xylylene modified by the substitution of chlorine atoms for two of the aromatic hydrogen atoms. Parylene D is similar in properties to Parylene C with the added abili.. |
|||
Volume Resistivity | 1.20e+17 ohm-cm | 1.20e+17 ohm-cm | |
Chengdu Polyster PPHA p-Hydroxybenzoic Acid Polymer PPHA is difficult to manufacture and brittle as well as low mechanical strength, its compounds have a higher mechanical strength and can be injection moulded. It can work without oil and its perform.. |
|||
Volume Resistivity | 1.20e+17 ohm-cm | 1.20e+17 ohm-cm | ASTM D257 |
DuPont™ Nomex® N196 Paper, 20 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |