Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.020 ohm-cm | 0.020 ohm-cm | Initial; Chomerics MAT-1002 |
Parker Chomerics CHO-FORM 5532 EMI Shielding Material One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. Cho-Form® 553.. |
|||
Volume Resistivity | <= 0.020 ohm-cm | <= 0.020 ohm-cm | Aged; Chomerics MAT-1002 |
Parker Chomerics CHO-FORM 5532 EMI Shielding Material One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. Cho-Form® 553.. |
|||
Volume Resistivity | 0.020 ohm-cm | 0.020 ohm-cm | Initial; Chomerics MAT-1002 |
Parker Chomerics CHO-FORM 5537 EMI Shielding Material Fast Curing Form-in-Place EMI Shielding Material. Cho-Form 5537 is a one component, moisture cured, electrically conductive, form-in-place EMI gasketing material. The formulation contains nickel-pla.. |
|||
Volume Resistivity | <= 0.020 ohm-cm | <= 0.020 ohm-cm | Aged; MIL-G-83528 Para. 4.6.15 |
Parker Chomerics CHO-FORM® 5518 Robotically Dispensed Gasketing Description: CHO-FORM® 5518 Two-component, thermal cure silicone system with Ag/Cu particle filler. Minimum cure temperature is only 85°C (185°F). Formulated for painted, plated or metalized plas.. |
|||
Volume Resistivity | 0.020 ohm-cm | 0.020 ohm-cm | Post Tensile Set; MIL-DTL-83528 Para.4.6.9 |
Parker Chomerics CHO-SEAL 1401 Conductive Elastomer High performance for non-corrosive environments; soft(45 Shore A) for low closure force where gasket geometry cannot be exploited; low tear strength; no fluid resistance. Molded and ExtrudedRoHS Com.. |
|||
Volume Resistivity | 0.020 ohm-cm | 0.020 ohm-cm | as supplied without pressure sensitive adhesive |
Parker Chomerics CHO-SEAL 1485 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Volume Resistivity | <= 0.020 ohm-cm | <= 0.020 ohm-cm | Cured; QAP-1017 |
Parker Chomerics Tecknit® 72-00008 Silver-Filled Epoxy System Description: This commercial grade, conductive epoxy is designed for use in bonding applications where good conductivity is required. When mixed in a ratio of 1:1.4 by volume or weight, the two comp.. |
|||
Volume Resistivity | <= 0.020 ohm-cm | <= 0.020 ohm-cm | |
Parker Chomerics Tecknit Teckfip™ FIP-N (LD) Formed in Place Conductive Elastomer Description: FIP-N is similar in performance to FIP-A elastomer and hence offers a good non-corrosive EMI shield in harsh conditions. This material is one of our more cost effective FIP compoundsInf.. |
|||
Volume Resistivity | <= 0.020 ohm-cm | <= 0.020 ohm-cm | |
Parker Chomerics Tecknit Teckfip™ FIP-N Formed in Place Conductive Elastomer Description: FIP-N is similar in performance to FIP-A elastomer and hence offers a good non-corrosive EMI shield in harsh conditions. This material is one of our more cost effective FIP compoundsInf.. |
|||
Volume Resistivity | 0.020 ohm-cm | 0.020 ohm-cm | |
Trelleborg Emerson & Cuming Eccobond® 64C Two-Component Nickel Filled Electrically Conductive Epoxy Adhesive Emerson & Cuming 64C Eccobond® Two-Component Nickel Filled Electrically Conductive Epoxy AdhesiveTwo component, nickel filled, electrically conductive epoxy adhesive. Room temperature cure. Good ba.. |
|||
Volume Resistivity | <= 0.020 ohm-cm | <= 0.020 ohm-cm | |
Epoxy Technology EPO-TEK® H24 Electrically Conductive Epoxy Product Description: EPO-TEK® H24 is a two component, electrically and thermally conductive epoxy adhesive designed for semiconductor die attach and hybrid micro-electronics assembly.Advantages & A.. |
|||
Volume Resistivity | 0.020 ohm-cm | 0.020 ohm-cm | |
Cotronics Duralco™ 127 400°F (200°C) Graphite Filled Epoxy One component, graphite filled epoxy for low cost production applications. Can be used with automatic dispensing equipment. |
|||
Volume Resistivity | 0.020 ohm-cm | 0.020 ohm-cm | Through plane |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC thermosets are the most .. |
|||
Volume Resistivity | 0.020 ohm-cm | 0.020 ohm-cm | Initial; Chomerics MAT-1002 |
Parker Chomerics CHO-FORM 5541 Conductive Form-In-Place Gaskets Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |