Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.015 ohm-cm | 0.015 ohm-cm | Post Tensile Set; MIL-DTL-83528 |
Parker Chomerics CHO-SEAL 1285 Conductive Elastomer Conductive Elastomer with Improved Corrosion Resistance. This conductive silicone elastomer features significantly improved corrosion resistance in salt spray environments over silver-plated copper-.. |
|||
Volume Resistivity | <= 0.015 ohm-cm | <= 0.015 ohm-cm | Post Tensile Strength; MIL-G-83528 |
Parker Chomerics CHO-SEAL 1285R Reinforced Conductive Elastomer Seal These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at.. |
|||
Volume Resistivity | 0.015 ohm-cm | 0.015 ohm-cm | Post Tensile Set; MIL-G-83528 Para.4.6.9 |
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shie.. |
|||
Volume Resistivity | <= 0.015 ohm-cm | <= 0.015 ohm-cm | Life Test/Post Tensile; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material Corrosion Resistant EMI Shielding Gasket. Through the use of new proprietary particle painting and elastomer compounding technology, CHO-SEAL® 1298 shielding elastomer offers a six-fold increase in.. |
|||
Volume Resistivity | <= 0.015 ohm-cm | <= 0.015 ohm-cm | |
Parker Chomerics Tecknit Consil®-R 856 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 856 offers the lowest durometer available for pure silver-filled elastomerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation.. |
|||
Volume Resistivity | <= 0.015 ohm-cm | <= 0.015 ohm-cm | Post Tensile Strength; MIL-G-83528 |
Parker Chomerics CHO-SEAL 1287R Reinforced Conductive Elastomer Seal These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at.. |