Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.0088 ohm-cm | 0.0088 ohm-cm | cured 1 hr @ 65°C |
Tra-Con Tra-Duct 916H01 Electronically Conductive Silver-Filled Epoxy TRA-DUCT 916H01 is an electronically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical .. |