Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.00060 ohm-cm | 0.00060 ohm-cm | Cured: 15 minutes at 25°C |
Resinlab® SEC1244 Silver Filled Epoxy Adhesive Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth.. |
|||
Volume Resistivity | 0.00060 ohm-cm | 0.00060 ohm-cm | cured 5 min @ 160°C |
Tra-Con Tra-Duct 2916 Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2916 is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good ele.. |
|||
Volume Resistivity | 0.00060 ohm-cm | 0.00060 ohm-cm | |
Trelleborg Emerson & Cuming Eccobond® 57C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive Emerson & Cuming 57C Eccobond® Two-Component Silver Filled Electrically Conductive Epoxy AdhesiveSilver filled, electrically conductive, room temperature curing, epoxy adhesive. Good thermal conduc.. |
|||
Volume Resistivity | 0.00060 ohm-cm | 0.00060 ohm-cm | cured 1 hr @ 110°C |
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2902 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical prop.. |