Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.000030 ohm-cm | 0.000030 ohm-cm | cure at 200°C |
Gwent Electronic Materials C2020425D1 Curable Silver Range This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive adhesive that combines good adhesion with excellent electrical properties.. |
|||
Volume Resistivity | 0.000030 ohm-cm | 0.000030 ohm-cm | |
Gwent Electronic Materials C2020711D3 Curable Silver Range This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive adhesive that combines good adhesion with excellent electrical properties.. |
|||
Volume Resistivity | 0.000030 ohm-cm | 0.000030 ohm-cm | |
ThyssenKrupp XABO® 355 Structural Steel This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Volume Resistivity | 0.000030 ohm-cm | 0.000030 ohm-cm | |
ThyssenKrupp XABO® 500 T Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Volume Resistivity | 0.000030 ohm-cm | 0.000030 ohm-cm | |
ThyssenKrupp XABO® 355 T Structural Steel This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Volume Resistivity | 0.000030 ohm-cm | 0.000030 ohm-cm | |
ThyssenKrupp XABO® 500 Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Volume Resistivity | 0.000030 ohm-cm | 0.000030 ohm-cm | |
ThyssenKrupp XABO® 460 Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Volume Resistivity | 0.000030 ohm-cm | 0.000030 ohm-cm | |
ThyssenKrupp XABO® 460 T Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |