Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 0.00000200 ohm-cm | <= 0.00000200 ohm-cm | |
Misumi Z3234 Chromium Copper Excellent mechanical strength and abrasion resistance at high temperatures. Used in welding electrodes, seam welding wheels, switch gears, electrode holder jaws, cable connectors, current carrying a.. |