Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.60e+16 - 3.60e+16 ohm-cm | 2.60e+16 - 3.60e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Volume Resistivity | 2.60e+16 - 3.60e+16 ohm-cm | 2.60e+16 - 3.60e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Volume Resistivity | 2.60e+16 - 3.60e+16 ohm-cm | 2.60e+16 - 3.60e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Volume Resistivity | 2.60e+16 - 3.60e+16 ohm-cm | 2.60e+16 - 3.60e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Volume Resistivity | 2.60e+16 - 3.60e+16 ohm-cm | 2.60e+16 - 3.60e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Volume Resistivity | 2.60e+16 - 3.60e+16 ohm-cm | 2.60e+16 - 3.60e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |