Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® PE 1295 PRE-ELEC PE 1295 is a dissipative thermoplastic compound based on PE-HD. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resistance bet.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Faradex MS002P PP (Asia Pacific) LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Faradex MS002P PP (Europe-Africa-Middle East) LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi.. |
|||
Volume Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D257 |
PolyOne Lubri-Tech™ SF-10CF/15T Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS CF10 A1 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA12 CF13 L 13% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 13% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and lubricatedInformation provided by TP Composi.. |
|||
Volume Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6/6 C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6/6 C14 BK 14% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC LNP STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific) LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX99620C PC LNP STAT-KON* DX99620C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX99620C PC (Asia Pacific) LNP STAT-KON* DX99620C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Asia Pacific) LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Volume Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66 LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Volume Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66 LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI (Asia Pacific) LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES HiFill® PPS 0237 A Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES HiFill® PPS 0334 A Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Absylux® CN-P Acrylonitrile-Butadiene-Styrene (conductive) Carbon-powder-filled conductive material with high strength and stiffness, and relatively high impact strength. This material is easily machined and fabricated into close tolerance finished parts. .. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Lennite® CN-P UHMW Polyethylene (conductive) Carbon-powder-filled, self-lubricating, conductive material with excellent abrasion-resistance and high impact strength. This material is light weight and easily machined, has good chemical and str.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Propylux® CN-P Polypropylene (conductive) Carbon-powder-filled lightweight material with good chemical resistance, extremely low water absorption level, and high impact resistance (no break, notched or unnotched). Rated UL94 V-0.Informatio.. |
|||
Volume Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Zelux® CN-P Polycarbonate (conductive) Carbon-powder-filled with high flexural strength and good thermal stability to 275F. The CN-P is UL94 V-0 rated at 0.030" and is thermoformable in thinner gauges (0.010"-0.060").Information provide.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Zelux® CN-SS Polycarbonate (conductive) CN-SS is filled with small non-sloughing stainless steel fibers. Has high flexural strength and good thermal stability to 275F. The CN-SS material has excellent impact strength. Information provid.. |
|||
Volume Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D150 |
Clariant Renol PCSP0008BK Polycarbonate, ESD Protection Data provided by Clariant Masterbatches |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Verton OX07411 PPS LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |